Studio Matrx — Material Reference

Material Comparison Sheet

India's interior material cheatsheet — plywood grades, finishes, hardware, countertops, flooring, paints, waterproofing, and city-wise price benchmarks for 2026.

12 Material Categories55+ Reference Items11 CitiesFree — No Sign-up
Indian interior material samples — ply, laminate, quartz, tile
12 MATERIAL CATEGORIES · 55+ ITEMS · 11 CITIESBWP PlyMDFLaminateVeneerQuartzGraniteTileWood FloorPU PaintAcrylicHardwareWaterproofCompare grade, price, durability, and warranty across every Indian brand.

Visual Compare

Vitrified vs wood vs marble vs Kota vs LVP — durability and lifespan per rupee.

Lowest Cost

₹0/sqft

Kota Stone

Longest Lifespan

0 yrs

Marble

Toughest

0/10

Vitrified Tile

Easiest Maintenance

0/10

Vitrified Tile

Side-by-side scoring (all axes 0–10, higher is better)

Affordability and Longevity are normalised within the selected category — the cheapest option scores 10 on Affordability, the longest-lasting scores 10 on Longevity. Durability, Maintenance ease and Install ease are absolute 1–10 scores from Studio Matrx's material specification database.

MaterialCost ₹/sqftDurabilityMaintenanceLifespan (yrs)Install Ease
Vitrified Tile₹1109/109/10257/10
Engineered Wood₹2757/105/10156/10
Marble₹3757/104/10404/10
Kota Stone₹559/108/10356/10
Luxury Vinyl₹1057/109/10129/10

Sample boards from real Indian projects

Plywood grade samples
Laminate sample swatches
Quartz and granite countertop edges
Tile and wood flooring options
Hettich Hafele Blum hardware

Specs Picked — Now See Them In Your Room

Choose your material spec, then render the room in DesignAI. Compare how BWP-ply walnut + quartz looks versus MDF teak veneer + granite — in your actual room photo.

Use your browser's Print dialog to save as PDF or print directly.

About this sheet

Curated from Amogh's professional material specification database. Rates and specifications are indicative for 2026 India market. Always verify with your contractor, architect, or interior designer before finalising specifications.