Mass Timber & Engineered Wood
Mastery check · Module 1
Understanding Wood as a Material
12 questions · pass mark 70%. Answer each, check it, and see where you stand before moving on.
Question 1 of 12
Single answer
At its most fundamental, wood is best described as:
A
A homogeneous solid, much the same in every direction
B
A natural fibre composite: hollow cellulose cells bonded and stiffened by lignin, running mainly one way
C
A pure crystal of cellulose with no internal structure
D
A random mix of fibres with no consistent direction
Check answer